I sold that 4011, so I got bored and built my larger plating station.
Some linkage
Bead blasted to get a finish.
I dunno how to do a step by step with this software.... dammit photobucket.
Anyway, I built a larger plating station. I like a more dull than shiny finish so I'm working on that. I shouldn't have strung all the pieces together as I got some shading as you can see in the later pictures.
I figure 25 milliamps per sq inch, so I ran this at 125 for about 8 minutes. After plated I dipped it in phosphoric acid, water washed, than dipped in yellow dichromate and rewashed with water. Just trying to get the larger station and rectifier figured out.